Colorfabb XT printing woes... Need Simplify3D tips/settings
Posted: Fri Jan 09, 2015 11:31 pm
Hi All,
First of all... I LOVE MY M2!!!!!!!!! I am in printing heaven, at least until late. I've been running only PLA since purchase (April 2014) and have had a grand time with almost all my prints until I met Colorfabb's XT.
I am in an emergency need of settings information for a wedding project I am printing, and we all know that we shall not miss wedding deadlines, right? The main reason for going with XT is the parts being printed are for outside use and we all know what happens to PLA in direct hot sunlight right? So enter Colorfabb XT filament.
I am using Simplify3D software, but my experience is limited, and I did manage to print a decent part a couple of times, but now using the same perimeters for some reason I get strings and drags etc. ad nauseam. Is there an 'apply these settings to current model' switch I don't know about? I just can't figure out why I got 2 decent prints before things went wonky.
Anywho... here is my dilemma with the Colorfabb XT filament. Recommended print temp is 240c to 260c...
1) Can my M2 print at those temps without meltdown? (my extruder block seems to rotate out of usual right angle alignment easily at the higher temps)
2) Can it continue to print one part right after the otherone or do I need a cool down time?
3) Does anyone on MakerGear Forum have experience with this particular filament?
4) Suggested settings?
5) Do I need a hotter/different extruder assy?
6) Where do I locate the perimeter speed so I can slow it down to get cleaner walls?
Here are the settings, from memory since I am at work until about 6:30pm PST. Settings are the default ones except what is noted. I gleaned this info from the post titled 'esun petg', posted by jdacal ยป Mon Nov 24, 2014 10:04 pm
Bed is level
Medium quality, 20% infill
Extruder temp = 250c (tried other temps too, some clumpy, some bubbles, some stringy)
Bed temp = 70c
Print Speed = 3200
Coast = OFF
Retract = 2mm (and 1.8mm)
Wipe = 5mm
I am not sure what hot end I have since this is my first venture into non PLA ill-printing filament situation, but my M2 was shipped to me last April 2014.
I was thinking of trying a little more 'retract' and a little 'coast' but not sure of how much.
Thanks in advance and if you could please reply asap with any info that might help I would be indebted!
First of all... I LOVE MY M2!!!!!!!!! I am in printing heaven, at least until late. I've been running only PLA since purchase (April 2014) and have had a grand time with almost all my prints until I met Colorfabb's XT.
I am in an emergency need of settings information for a wedding project I am printing, and we all know that we shall not miss wedding deadlines, right? The main reason for going with XT is the parts being printed are for outside use and we all know what happens to PLA in direct hot sunlight right? So enter Colorfabb XT filament.
I am using Simplify3D software, but my experience is limited, and I did manage to print a decent part a couple of times, but now using the same perimeters for some reason I get strings and drags etc. ad nauseam. Is there an 'apply these settings to current model' switch I don't know about? I just can't figure out why I got 2 decent prints before things went wonky.
Anywho... here is my dilemma with the Colorfabb XT filament. Recommended print temp is 240c to 260c...
1) Can my M2 print at those temps without meltdown? (my extruder block seems to rotate out of usual right angle alignment easily at the higher temps)
2) Can it continue to print one part right after the otherone or do I need a cool down time?
3) Does anyone on MakerGear Forum have experience with this particular filament?
4) Suggested settings?
5) Do I need a hotter/different extruder assy?
6) Where do I locate the perimeter speed so I can slow it down to get cleaner walls?
Here are the settings, from memory since I am at work until about 6:30pm PST. Settings are the default ones except what is noted. I gleaned this info from the post titled 'esun petg', posted by jdacal ยป Mon Nov 24, 2014 10:04 pm
Bed is level
Medium quality, 20% infill
Extruder temp = 250c (tried other temps too, some clumpy, some bubbles, some stringy)
Bed temp = 70c
Print Speed = 3200
Coast = OFF
Retract = 2mm (and 1.8mm)
Wipe = 5mm
I am not sure what hot end I have since this is my first venture into non PLA ill-printing filament situation, but my M2 was shipped to me last April 2014.
I was thinking of trying a little more 'retract' and a little 'coast' but not sure of how much.
Thanks in advance and if you could please reply asap with any info that might help I would be indebted!